Customization: | Available |
---|---|
Application: | Local Communication Cable, Coaxial Cable, LAN Cable, Long Distance Symmetric Cable, RF Cable, Submarine Cable |
Conductor Material: | BC/CCS/CCA/TC/CU/CCAG |
Still deciding? Get samples of US$ 0/Piece
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Construction Parameters: | ||
Nomial diameter Φ /mm | 0.2mm | |
Diameter difference ±mm | ±0.004mm | |
Copper content % | 27 % | |
Density (20 ºC) g/cm3 | 3.3 g/cm3 | |
Intensity test of the soft state ≥N | ≥3.7 N | |
Tensile strength of soft-state≥N/mm2 | ≥120 N/mm2 | |
Hard measured intensity ≥N | ≥8.4 N | |
Tensile strength of hard-state≥N/mm2 | ≥270 N/mm2 | |
Electrical Characteristics: | ||
Resistivity (20ºC) ≤Ω.km/mm2 | ≤27.5 Ω.km/mm2 | |
Measured resistance (20 ºC) ≤Ω/km | ≤875Ω/km | |
Conductivity (20 ºC) ≥% | ≥63 % | |
Soft-state elongstion≥% | ≥10 % | |
Hard elongation≥% | ≥12 % | |
Product Inspection: | ||
Inspection Item | Standard Requirement (ASTM B 566-93) | Inspection Result |
1. Surface | Bright, Clean, no flaw | OK |
2. Diameter (mm) | 0.2(+/-0.004mm) | OK |
3. Tensile Strength (N/mm2) | ≥120 N/mm2 | OK |
4. Elongation (%) | ≥10 % | OK |
5. Density (g/cm3) | 3.3 (±0.03)g/cm3 | OK |
6. Resistivity (20ºC) ≤Ω.km/mm2 | ≤27.5 Ω.km/mm2 | OK |
7. Conductivity (%IACS) | ≥63 % | OK |
Conclusion | Pass | |
Order Informations: | ||
Technical Parameter | based on customer's requirements | |
Package | Please advise the spool size or your special requirements | |
Delivery time | Normally 20-25 days after received the deposit. | |
Application | braid shielding & cable conductor (single or stranded) for coaxial cable, power cable, signal cable, network cable, data cable, enameled wire etc | |
More informations | please contact with us. |
COPPER WIRE
|
CCAM WIRE
|
ALUMINUM WIRE
|
|
Copper Percent in Volume(%)
|
100
|
15
|
0
|
Density(g/cm3)
|
8.89
|
3.50
|
2.70
|
Length Comparison based on same Diameter and same weight
|
1:1
|
2.5:1
|
3.29:1
|
Resistivity(ohm.mm2/m)
|
0.01724
|
0.035
|
0.02740
|
Tensile strength(Mpa)
|
215-265
|
≥160
|
68-107
|
Elongation(%)
|
≥20
|
≥10
|
≥15
|